TECHNET Archives

September 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
"Alderete, Michael" <[log in to unmask]>
Date:
Tue, 29 Sep 1998 10:43:16 -0700
Content-Type:
text/plain
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Alderete, Michael" <[log in to unmask]>
Parts/Attachments:
text/plain (63 lines)
Jim-

I think I've read that Scanning Acoustic Microscopy (SAM) may not
reliably detect faulty or cold solder joints, BUT it may be worth
running by the people at Sonoscan Corp:

in San Jose, CA 408-456-0204

in Bensenville, IL 630-766-7088, 800-950-2NDT

-Michael Alderete



You wrote...
------------------------------

Date:    Tue, 29 Sep 1998 07:48:00 -0400
From:    Jim Marsico 516-595-5879 <[log in to unmask]>
Subject: Re: ASSY: BGA FAILURES

Well, how about it!  Does anyone have any experience using ultrasound to
detect
cracked solder joints?  Does anyone know of a testing lab that can
perform this
function?

Thanks again...

Jim Marsico


Mark wrote:

Dear Jim

This may be a very stupid idea, but what about using ultrasound?

I believe they use ultrasound to detect microscopic fractures in
mechanical
assembly's and the joint between the CBGA and the solder ball is
mechanical.

I don't know what the ultrasound would do to the chip or the wire bonds
but
it may be worth some more inquiries to the component manf.

I would be very interested to read how you got on.

------------------------------

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2