Bill,
I would love to but I really don't have alot.
All of the information technetters gave me was passed on to the
Japanese at my company. What I did find out was that It showed
up in the original design. My understanding is that this is a design
issue.
I was told that they are now working on a new design
for the problem area.
( This is a new product not yet on the market )
So we are not in any trouble ( Knot on Wood )
This is just one of many bugs in the
progress of improvment
Sorry I know it's not what you really wanted
but It's really all I have
Nancy
>>> Bill Davis <[log in to unmask]> 10/06/99 01:53PM >>>
Nancy- just for the edification of all who responded- can you share with us
what the root cause of your problem was- might keep some of us from
repeating the same mistake...
thx
> Bill Davis, Ph.D.
> S3, Inc.
> Senior Scientist
> 408.325.7868
> [log in to unmask]
>
>
-----Original Message-----
From: Nancy Trumbull [mailto:[log in to unmask]]
Sent: Tuesday, October 05, 1999 10:29 AM
To: [log in to unmask]
Subject: [TN] Electrical Migration Closed
Hi Everyone again
I want to say thank you all very much.
I passed all of the information on to management.
They have informed me that they have pinned down the problem.
And are now working on resolving the issue.
I received detailed information that was helpful
in the evaluation of the real problem.
My involvement with this particular issue was gathering of information.
thanks to you ( all the technet who replied )
I can through.
Again I thank you
Nancy
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|