JW,
The answer is no. The OSP is supposed to last up to 6 months. Once you have process the PWB through the oven the first time the OSP is gone and then oxidation will start to occur so you want to process as soon as possible. Unless you have a harsh environment (high sulfur) you should be good for a few days.
Russell Nowland
Alcatel-Lucent
Advanced Manufacturing Engineer
Address: 14000 Quail Spring Parkway, Suite 300
Oklahoma City, OK 73134
email: [log in to unmask]
Desk: 405-302-1660
Cell: 405-203-0034
Fax: 405-302-1622
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of J W
Sent: Monday, July 19, 2010 7:45 AM
To: [log in to unmask]
Subject: [TN] OSP Coating
Hi,
Is it true when a PCB is OSP coated it needs to be populated within 24 hrs
of opening the package due to oxidation?
Thanks,
JW
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|