TECHNET Archives

August 2011

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Richard Hatano <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Richard Hatano <[log in to unmask]>
Date:
Wed, 31 Aug 2011 14:52:00 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (108 lines)
Hi Mark,

I should have said that I do normally tent the vias (with soldermask on the
far side from slug).
This would help reduce thieving, which as Dave notes should be avoided.  I
remember following a mfr. white paper on thermal conduction of pth, and was
surprised at how few were needed.  Tenting the vias spoils some of their
thermal use, but it's a trade-off, and I've never been presented with solder
or thermal problems caused by the vias used under the part with the scheme I
described.

Richard

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Wednesday, August 31, 2011 2:12 PM
To: [log in to unmask]
Subject: Re: [TN] QFN with solder slug

Hi Mark - if you leave the thermal vias open then the solder will thieve 
down them leaving the center pad "solder starved". I recommend you use 
some fabrication format which permits the vias not allowing solder to 
thieve - aka either capping them or filling them. The IPC-7093 standard on 
Bottom Termination Components also may have some helpful information.

Dave Hillman
Rockwell Collins
[log in to unmask]




Mark Larson <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
08/31/2011 02:52 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Mark Larson <[log in to unmask]>


To
<[log in to unmask]>
cc

Subject
[TN] QFN with solder slug






I am curious how others are handling these parts for soldering. Do you 
leave the thermal vias in the slug covered or uncovered with solder mask? 
Do you fill with anything? What size hole on a 62 mil board? Tie to all 
GND planes or just the back side? Thermal relief the via or bury it in the 
plane?

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2