by ipc.org (Smail3.1.28.1 #2) id m0wIE0N-000Bj1C; Fri, 18 Apr 97 08:47 CDT
Old-Return-Path:
Date:
Fri, 18 Apr 97 09:39:27 EST
Precedence:
list
X-Loop:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/12104
TO:
Return-Path:
<TechNet-request>
From [log in to unmask] Fri Apr 18 10:
30:59 1997
Resent-Message-ID:
<"SZRbV.0.p8C.UjtLp"@ipc>
Subject:
From:
"Tom Cooper" <[log in to unmask]>
Resent-From:
Message-Id:
Parts/Attachments:
text/plain (52 lines)
     Dan,
        This is not an answer to your repair question, but an inquiry of my 
     own. We are about to assemble some boards using TBGA's and was 
     wondering if these packages require pre-baking as do PQFP's to remove 
     moisture. In reading about TBGA technology, I find no mention of 
     pre-baking or moisture sensitivity ratings. Please advise.
     
     Thank you in advance,
     [log in to unmask]  


______________________________ Reply Separator _________________________________
Subject: TBGA's on "big boards"
Author:  [log in to unmask] at INTERNET
Date:    4/17/97 11:21 AM


we are currently building some 18" by 20" product 
with up to 4 500+ I/O TBGA's......The production 
process is ok....but we have some difficulty 
during repair....Preheat profile control is a 
critical parameter...does anyone have experience 
with TBGA repair on big boards?  What repair 
platform should I investigate?
     
thanks
     
dan
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   * 
* with <subject: subscribe/unsubscribe> and no text in the body.          * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2