Hello Patrick,
Do you really want to fix it or do you want to experiment?
Using a soldering iron is not a good idea because the heat will never
transfer from the top of the component to all of the spheres or the PCB.
If you were to use hot-air and a thermocouple you might have success since
an SODIMM has such a low mass and the memory BGAs are so thin.
Then again, if you don’t bake-out the moisture, you might have latent
component and/or PCB failures.
Thank you,
David Tremmel
872 S. Milwaukee Ave, #253
Libertyville, IL 60048
847 858-5540 - Phone
www.ValuRecovery.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Goodyear, Patrick
Sent: Monday, October 17, 2011 12:10 PM
To: [log in to unmask]
Subject: [TN] Reflow of BGA
Ok gang, I'm stretching my limits here.
Does anyone have experience with hand reflow of BGA? I have never tried
it. Does one use a hot jet or can it be done with the iron to the
component.
Most notably on a SODIMM, one of the memory chips has a bad connection,
looks like 3 rows per side of 8 per row.
Pat
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|