TECHNET Archives

February 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
"Foote, Jeffery" <[log in to unmask]>
Date:
Thu, 14 Feb 2002 08:18:01 -0800
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Foote, Jeffery" <[log in to unmask]>
Parts/Attachments:
text/plain (82 lines)
Rudy, You are correct the boards do not have buried vias, but the
delamination does not necessarily locate adjacent to a hole.  Tests on bare
boards showed that they do occur primarily at one end of the PWB on layer 5
of 8.  The delaminations occur on the "sawtooth" side of the copper.
Additionally, examination through the laminate on the secondary side (layer
8) revealed black patchy areas over large land patterns or ground planes on
layer 7.  These also occur on the sawtooth side of the copper.  Although
these areas have not delaminated, I have confirmed that the laminate resin
does not bond to these areas and EDS showed the same presence of sulfur and
tin that was observed on the delaminated surfaces.  Do you know what
chemical preparation the sawtooth side of the copper is exposed to in order
to improve adhesion?

Thanks Rudy for your time.
Best Regards,
Jeff

-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Wednesday, February 13, 2002 3:33 PM
To: [log in to unmask]
Subject: [TN] Delamination


In a message dated 2/13/02 2:58:07 PM Pacific Standard Time,
[log in to unmask]
writes:

<< I am looking for some information regarding the preparation of copper
foil
 for adhesion to internal laminate layers in the construction of PWBs.  I am
 presently experiencing delamination of the copper from the laminate prepreg
 on an internal layer after IR reflow exposure.  EDS of the delaminated
 surfaces showed localized, high-concentration of sulfur and tin on the
 copper surface >>

Jeff:  I assume that this delamination is occuring adjacent to drilled
holes?
 These are not buried via boards are they?

Rudy Sedlak
RD Chemical Company

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----


The information contained in this email message may be privileged and is
confidential information intended only for the use of the recipient, or any
employee or agent responsible to deliver it to the intended recipient. Any
unauthorized use, distribution or copying of this information is strictly
prohibited and may be unlawful.

If you have received this communication in error, please notify the sender
immediately and destroy the original message and all attachments from your
electronic files.

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2