Hi Craig,
How many solder bumps on how many PCBs?
If it's just a few (more than 50 will drive you insane) try putting a tiny
bit of paste flux down with a needle on the pad only. Then wipe off the
needle leaving a trace of flux on it. Use the needle to pick up balls from
a jar and place them one at a time on the pads. You will need a good
microscope. Then reflow the PCB. If the flux goes from pad to pad then so
will the balls.
If it is a lot then send me a personal e-mail and I'll do my sales pitch.
How large is the PCB? Is it already loaded/populated?
Hope this helps
-----Original Message-----
From: Craig McGlinchy <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Tuesday, September 01, 1998 2:43 PM
Subject: [TN] Solder Bumping
>Hi All,
>
>I am trying to find out if it is possible to get solder bumps (as on a bga)
>place on a PCB, the pitch of the solder bumps would be 0.8mm, and the
>diameter of the bump approx 0.5mm.
>
>Thanks
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|