I am not sure that is solder defect. It almost looks like what you can get
out of the copper plating tanks if the filtering is not working properly.
Scott Westheimer
----- Original Message -----
From: "Bissonnette, Jean-Francois" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, January 09, 2004 3:32 PM
Subject: [TN] Inner Wall Defect
Hi technetters,
We recently received flex cables with PTH that have holes blocked by some
kind of solder
webing. I've asked Steeve Gregory to post them on his web site. I would
like to have
opinions from the experts out there. Even though the supplier has been
asked many times
to correct the process the flex circuits often have that defect... Any idea?
The pictures are at: http://www.stevezeva.homestead.com under Inner Wall
Defect.
Thanks!
Jean-François Bissonnette
Vérificateur, Contrôle de la Qualité
Électronique
Produits et Procédés
Vapor Rail Inc.
10655 Henri-Bourassa O.
St-Laurent, Qc
H4S 1A1
(514) 335-4200 x2021
(514) 335-4231 fax
***** CONFIDENTIALITY NOTE *****
The content contained in this e-mail transmission is legally privileged and
confidential information intended only for the use of the individual or
entity named herein. If the reader of this transmission is not the intended
recipient, you are hereby notified that any dissemination, distribution, or
copying of this transmission is strictly prohibited.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|