TECHNET Archives

March 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 13 Mar 2012 14:42:33 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Charlie Pitarys <[log in to unmask]>
Subject:
MIME-Version:
1.0
Message-ID:
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="us-ascii"
From:
Charlie Pitarys <[log in to unmask]>
Parts/Attachments:
text/plain (36 lines)
I have these PCB's (mixed technology) in house, used for an automotive under
hood application. In several spots on the board are these array of holes. On
the A-side a smt component like a thyristor will cover up the array.
What are these there for? 
The wave flux residue is proving tenacious to effectively clean out of every
via. Especially with the old school cleaning tool at this account.

Some of the vias are clear but some have solder filling or partially filling
them. These are now also filled with wave flux.
Below is a link to a picture of the array.
http://i123.photobucket.com/albums/o319/dartfrogmts/Kyzen/A-Side00140xFCR145
F20min-1.jpg

I'll get them clean but curious as to why these are on the board.
Thanks in advance

Charlie




CONFIDENTIAL
The content of this message, including any attachments, may contain
privileged and/or confidential information proprietary to Kyzen and is
intended only for the named addressees. If you are not the intended
recipient, you may not disseminate, distribute or copy this email. Please
notify the sender immediately by email if you have received this email in
error and delete this email from your system.



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2