TECHNET Archives

September 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
TechNet Mail Forum<[log in to unmask]>
Subject:
From:
Date:
Sat, 6 Sep 1997 10:59:04 -0400
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (15 lines)
Hi Glenn,
I do not have a copy of this reference, but from my experience and the rest
of the literature I would rather strongly feel that the acceleration model
given in the article represents more wishful thinking than reality. So my
advice is be careful.

Werner Engelmaier
Engelmaier Associates, Inc.
Electronic Packaging, Interconnection and Reliability Consulting
23 Gunther Street
Mendham, NJ  07945  USA
Phone & Fax: 973-543-2747
E-mail: [log in to unmask]