Hi Cal:
The general consensus everywhere I have been is that ultrasonic cleaning will damage the wirebonding from the ICs to the carrier pads. Those gold or silver wires used are thinner than hair and, if vibrated, there is a potential of breakage. As far as cleaning, it will do a better job than agitation or spray. It does a good job in cleaning in between small crevices. It is my understanding that someone built a cloth washer using the ultrasonic principle and does not need detergent.
Regards,
Ramon
-----Original Message-----
From: Cal Driscoll [mailto:[log in to unmask]]
Sent: Thursday, June 17, 2004 11:40 AM
To: [log in to unmask]
Subject: [TN] Cleaning PCB's With Ultrasonics...
Hello All-
Recently I was away on Holiday and when I came back....there was a Branson
Utlrasonics system being used to clean our newly assembled PCB's. The
machine is a standard ultrasonics (parts cleaner I call it) bath using a
general cleaner/degreaser.
Facts:
Our process is:
- No clean
- double sided
- mix technology
- Discrete (tants, Chips resistors)
- BGA's
- QFPs
- PLCC's
- ASICS
- Connectors
- Headers
- Electrolytic Caps
Concerns:
- Ultrsonics damaging internals on IC's
- Residues left after cleaning
- Effects on Programmable IC's
- .....Just General over all reliability.
I have huge concerns on the over all cleanliness and reliability. Any info
supporting or declining this is of interest.
Thanks in advance,
Cal
Caldon Driscoll
Program Manager, Circuit Board Manufacturing
CTDI
1373 Enterprise Drive
West Chester, PA 19380
610-793-8098
WWW.CTDI.COM
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|