TECHNET Archives

March 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
David Douthit <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, David Douthit <[log in to unmask]>
Date:
Thu, 10 Mar 2005 17:28:30 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (55 lines)
Bob,

That's the whole idea! There are none. There some recommendation that
are very general in nature but there is no longer a "one size fits all"
testing standard. You must determine the end use environmental
conditions and life warranty requirements for each product and test
accordingly. You must learn to correlate testing to field conditions
(not easy - you need a lot of experience).
This is causing serious soul (sole for Dewey) searching for Pb free builds!

Good luck!

David A. Douthit
Manager
LoCan LLC

bob wettermann wrote:

>Dear Technetters:
>
>In reviewing the myriad of BGA reliability tech papers there seems to be little commonality in the type of test protocols. There are tests that are industry specific, device vendor specific and customer specific.
>
>What guidance in terms of minimum mechanical solder joint strength and reliability testing would the knowledgeable designers (for CLASS II products)have for us? (We are NOT designers of circuit boards, systems or devices). Any test protocol standards? What would be the acceptance criteria for pass/fail be? What type of measurements would be required as a minimum?
>
>Best Regards
>Bob Wettermann
>
>
>Bob Wettermann
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
>-----------------------------------------------------
>PH 847-767-5745
>
>
>
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2