TECHNET Archives

March 2011

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Steven Kelly <[log in to unmask]>, TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 17 Mar 2011 10:03:57 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
<52135AE4151D8343B16989B2BFBED7DA1D34EEA1FD@pfc-dc01>
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (57 lines)
Here you go, sir.
http://www.taconic-add.com/pdf/technicalarticles--effectsofsurfacefinish.pdf


-----Original Message-----
From: Steven Kelly [mailto:[log in to unmask]] 
Sent: Thursday, March 17, 2011 8:46 AM
To: Stadem, Richard D.; TechNet E-Mail Forum
Subject: RE: Signal loss

Thanks Richard,
Is there a number or % I can hang my hat on? Regards Steve

-----Original Message-----
From: Stadem, Richard D. [mailto:[log in to unmask]] 
Sent: March-17-11 9:44 AM
To: TechNet E-Mail Forum; Steven Kelly
Subject: RE: Signal loss

Yes. Absolutely. At that frequency the signal skin effect is very pronounced, and having a nickel finish can prove to be very lossy. You may wish to investigate immersion silver finish instead.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Kelly
Sent: Thursday, March 17, 2011 8:30 AM
To: [log in to unmask]
Subject: [TN] Signal loss

Good Day To All,
We recently fabricated a surface microstrip flex circuit with 50 ohm +/- 2.5 ohms (results were good). The impedance traces were not covered with solder mask or coverlay but were plated with ENIG. The next part is where I need the help. The circuit runs at 20-26 Ghz. Customer says the return losses from the S-parameters measurements are good but the insertion losses are not (quite frankly I have no idea what this means) . Could the nickel plating be causing this issue?
Thanks.
Steve Kelly

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2