TECHNET Archives

July 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 11 Jul 2007 14:50:13 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Tom P. Hummel" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
"Tom P. Hummel" <[log in to unmask]>
Parts/Attachments:
text/plain (42 lines)
Fellow TechNetters,

 

We are experiencing a white residue on the solder side of some boards
after going through our wash system.  We are wave soldering the boards
on a SeHo wave solder machine using Aim NC-264-5 no clean flux.  The
boards have some additional components installed by hand using water
soluble flux/solder.  The boards are then run through our Aqueous
Technologies SMT series board washer.  When they complete the drying
cycle, there is a white residue on the solder side of the boards that is
very difficult to remove.  Has anyone else seen this residue from
washing a board after using no clean flux?  Does anyone have any
recommendations to help eliminate the residue?

 

 

Thomas P. Hummel

Carlton Industries Corp

 

 

 

 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2