Rick - at Photocircuits we consider Flash gold as electrolytic 5 microinches
in thickness, same approximate thickness as ENIG but can be a totally
different species - Au purity being a consideration. After reflow is the
gold dissolved from the pad?
Regards
Gerard O'Brien
Photocircuits Corp
-----Original Message-----
From: Rick Thompson [mailto:[log in to unmask]]
Sent: Monday, January 27, 2003 1:58 PM
To: [log in to unmask]
Subject: [TN] Immersion Gold vs Flash gold finish with Lead-free?
Can someone tell me what the difference is between immersion gold and flash
gold as a board finish? Is the 'flash' process a different type of plating
process? Also, has anyone had any experience using Lead-free solder paste
on a Flash gold finish? We're currently having some solder wetting issues
with lead-free on flash gold where some of the pads on the boards exhibit
complete lack of any wetting. It almost looks like what you get when you
reflow solder paste on a ceramic substrate, where the solder just balls up.
Is this an inherent problem with flash gold or do I have some kind of
abnormal processing issue at the board vendor?
Thanks in advance.
Rick Thompson
Sr. SMT Process Engineer
SMTEK International, Inc.
+1 (805) 532-2800
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|