IPC-2222, 9.2.2, Table 9-3.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Roberts, Jon (SA-1)
Sent: Tuesday, February 23, 2010 6:46 AM
To: [log in to unmask]
Subject: [TN] LEAD TO HOLE RATIO QUESTION
I was trying to find in IPC 2200 series where the lead to hole ratio is
discussed. I remember we would provide to contractor instructors the
requirements. That is going back to the WS5626 days. Can you direct me
where to find that information. I am looking for double side-multilayer
boards for meeting Class 3 of IPC J-Std-001.
Thanks, Jon
This communication is intended only for use by the addressee(s) named
herein and may contain business confidential and/or legally privileged
information. If you are not the intended recipient of this e-mail, you
are hereby notified that any dissemination, distribution, disclosure or
copying of this e-mail and its contents is strictly prohibited. If you
have received this e-mail in error, kindly notify the sender by replying
to this message. In addition, please permanently delete the message and
any attachments without copying or disclosing the contents. Thank you
for your cooperation.
THIS DOCUMENT AND/OR SHIPMENT MAY CONTAIN COMMODITY ITEMS, SOFTWARE OR
TECHNICAL DATA THAT IS CONTROLLED BY U.S. EXPORT LAW, AND MAY NOT BE
EXPORTED OUTSIDE THE UNITED STATES OR TO NON U.S. PERSONS WITHOUT THE
APPROPRIATE EXPORT LICENSE FROM EITHER THE U.S. DEPARTMENT OF STATE OR
DEPARTMENT OF COMMERCE.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
--------------------------------------------------------------------------------
We value your opinion! How may we serve you better?
Please click the survey link to tell us how we are doing:
http://www.craneae.com/ContactUs/VoiceofCustomer.aspx
Your feedback is of the utmost importance to us. Thank you for your time.
--------------------------------------------------------------------------------
Crane Aerospace & Electronics Confidentiality Statement:
The information contained in this email message may be privileged and is
confidential information intended only for the use of the recipient, or any
employee or agent responsible to deliver it to the intended recipient. Any
unauthorized use, distribution or copying of this information is strictly prohibited
and may be unlawful. If you have received this communication in error, please notify
the sender immediately and destroy the original message and all attachments from
your electronic files.
--------------------------------------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|