TECHNET Archives

1996

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
[log in to unmask] (MR JIM R ZANOLLI)
Date:
Tue, 6 Aug 1996 08:00:16, -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (24 lines)
-- [ From: Jim Zanolli * EMC.Ver #2.10P ] --

Does anyone have any ideas on how to solder thru-hole connectors
without the extra step of wave soldering? In many cases a sufficient
volume of solder cannot be achieved by applying solder paste to the
hole. 

In another case the connector has long .485" .025 square tails that
must have  gold plating to allow mating to another connector after
soldered to PCB -- and therefore cannot even be wave soldered. Are
there any alternatives to laborious hand soldering or solder donuts?

Does the term "intrusive reflow" define the soldering of thru-hole
leads by paste in the hole and reflow?

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2