Part 2 which I left off. Sorry for double post.
Alternatively:
Could this be a mechanical change? Maybe the Di water droplets are different
sized compare to the town water. Is the surface tension of water affected by
hardness? When upgrading to DI did you take the opportunity to change the
pumps or filters or something which has changed the droplet nature?
Regards
Mike
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Mike Fenner
Sent: Wednesday, January 05, 2011 8:04 PM
To: [log in to unmask]
Subject: Re: [TN] Deionized water in misting fans and static electricity
HNY everyone
Normal humidity is made from DI water, that's how it got there, so the use
of DI water shouldn't make any difference, but Steve says it does, so here
is my hypothesis.
The object of the water mister is presumably to generate a stream of
humidified air which would mimic natural humidity.
But the RH won't be changed till the water is in vapour form. Till then you
have dry air with lumps of water passing by.
So could it be that the mister is making a continuing stream of droplets
each one tribocharged. It would therefore be like a charge conveyor belt
(think Van de Graf generator rather than thunderstorm),
Maybe you have to a water evaporator or heater or something?
Regards
Mike
ü Please consider the environment before printing this e-mail
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Paul Edwards
Sent: Wednesday, January 05, 2011 6:45 PM
To: [log in to unmask]
Subject: Re: [TN] Deionized water in misting fans and static electricity
Not because of the deionized water as much as the water itself...
Space charge collects on water droplets at emission point and due to
movement... Then the chargeable particulate generates current due to a delta
V in potentials...Think thunderstorms...
Paul
Paul Edwards
Process/Quality Engineering
Surface Art Engineering
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Wednesday, January 05, 2011 10:32 AM
To: [log in to unmask]
Subject: [TN] Deionized water in misting fans and static electricity
This may be an off the wall question but here goes.
We have some misting fans that we use for humidification that we've just
recently put in a deionized water source for.
Now it seems that there's a static charge being generated at the fans that
I've never noticed before. Could it be possible that we're generating a
charge at the fans because of the DI water?
Steve
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
============================================================================
==
This email and any attachments thereto may contain private, confidential,
and
privileged material for the sole use of the intended recipient. Any review,
copying,
or distribution of this email (or any attachments thereto) by others is
strictly prohibited.
If you are not the intended recipient, please contact
[log in to unmask]
immediately and permanently delete the original and any copies of this email
and
any attachments thereto.
============================================================================
==
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
***This email, its content, and any files transmitted with it, are intended
solely for the addressee(s) and may be legally privileged and/or
confidential. If you are not the intended recipient, please contact the
sender by return and delete the material from any computer. Any review,
retransmission, dissemination, or other use of, or taking of any action in
reliance upon this information by persons or entities other than the
intended recipient is prohibited.
Messages sent via this medium may be subjected to delays, non-delivery, and
unauthorized alteration. This email has been prepared using information
believed by the author to be reliable and accurate, but Indium Corporation
makes no warranty as to accuracy or completeness. Indium Corporation does
not accept responsibility for changes made to this email after it was sent.
Any opinions or recommendations expressed herein are solely those of the
author. They may be subject to change without notice.***
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|