TECHNET Archives

July 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Optiprint AG <[log in to unmask]>
Date:
Mon, 5 Jul 1999 08:56:27 +0200
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, TOE /Torben Østeraa <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="ISO-8859-1"
From:
TOE /Torben Østeraa <[log in to unmask]>
Parts/Attachments:
text/plain (40 lines)
Simon, 

About 10 years ago, this product was sold by 

'Climax Speciality Metals' in Ohio
+1 44117 1117 ( obsolete?)

you could probably get help from 

Climax Molybdenum GmbH
Duesseldorf
+49 211 864 64 0
fax +49 211 64 64


regards

Toben Østeraa
Printca AS

>>-----Original Message-----
>>From: Optiprint AG [mailto:[log in to unmask]]
>>Sent: Monday, July 05, 1999 8:15 AM
>>To: [log in to unmask]
>>Subject: [TN] Supplier of Molybden?
>>
>>
>>Hi.
>>
>>I am looking for a supplier of Cu-Molybden-Cu Material. 
>>Thickness 0.1mm.
>>Can anyone help?
>>
>>Thank you in advance.
>>
>>Best regards.
>>Optiprint AG
>>Simon Huetter
>>