TECHNET Archives

June 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Date:
Thu, 17 Jun 2010 10:55:25 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Craig Sullivan <[log in to unmask]>
Subject:
From:
Craig Sullivan <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
<001501cb0e19$e309e980$a91dbc80$@com>
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (317 lines)
"I don't know why Humiseal quit making their tape, it was one of the best

tapes I ever used. But then they just stopped making it for some reason."

 

Humiseal never made the tape. They procured it from St. Gobain and
renumbered it with their own part number. St. Gobain had severe production
issues with this tape and as such Humiseal got tired of dealing with it.
There was a company in Florida that was cutting it for them, but he tripled
his prices so we found another supplier.

 

The part number is M797 from St. Gobain and is still readily available from
various suppliers. We get ours from http://www.robertmckeown.com/ Just be
sure to tell them to cut it without silicone. 

 

 

Craig Sullivan

Manufacturing Engineer

MPL Incorporated

P: 607.266.0480

F: 607.266.0482

[log in to unmask]

 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Thursday, June 17, 2010 8:38 AM
To: [log in to unmask]
Subject: Re: [TN] 3M tape/adhesive concern

 

Hi Linda!

 

 

 

Gosh, I'm sorry I didn't get these posted earlier. I was planning to as soon

as I got them, but I got busy doing something else and forgot about your

request. Thanks for reminding me.

 

 

 

Anyways, here's your pictures:

 

 

 

http://stevezeva.homestead.com/adhesive.JPG

 

 

 

http://stevezeva.homestead.com/adhesive_2.JPG

 

 

 

http://stevezeva.homestead.com/paper_debri.JPG

 

 

 

http://stevezeva.homestead.com/under_button.JPG

 

 

 

I know it's bit of a challenge to find good conformal coat masking tape that

doesn't leave residues and debris, especially if you bake the boards to tack

cure the coating.

 

 

 

I don't know why Humiseal quit making their tape, it was one of the best

tapes I ever used. But then they just stopped making it for some reason.

 

 

 

Steve

 

 

 

From: Linda Langley [mailto:[log in to unmask]] 

Sent: Monday, June 14, 2010 2:43 PM

To: Steve Gregory

Subject: FW: 3M tape/adhesive concern

 

 

 

Steve,

 

Could you please post these pictures? We are having problems where there is

adhesive is sticking to the board when we pull the tape off.

 

Does anyone know if this would be a problem according to IPC? Would this be

considered Particulate Matter? Any info will be greatly appreciated.

 

 

 

Thanks

 

 

 

Linda Langley CIT

 

Training Specialist

 

Jabil Circuit

 

248-292-6176

 

From: Klara Szalay 

Sent: Tuesday, June 08, 2010 8:23 AM

To: Linda Langley

Subject: RE: 3M tape

 

 

 

I am sorry, I had to leave early yesterday. Here are some pictures of what

you looked at yesterday. Let me know if you need additional pictures.

 

Klara

 

 

 

From: Linda Langley 

Sent: Monday, June 07, 2010 10:37 AM

To: Klara Szalay

Subject: 3M tape

 

 

 

Klara,

 

Can you send me a picture of the tape concern?

 

 

 

Linda Langley CIT

 

Training Specialist

 

Jabil Circuit

 

248-292-6176

 

 

 

______________________________________________________________________

This email has been scanned by the MessageLabs Email Security System.

For more information please contact helpdesk at x2960 or [log in to unmask] 

______________________________________________________________________

 

---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815

-----------------------------------------------------

 



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2