-- [ From: Tony Bugeja * EMC.Ver #2.5.02 ] --
At my previous company we used a Thermotron with humidity for curing Silicon
3140 on 6x9 PCBA's, this reduced the cycle time for cure in half.
Subject: [TN] Moisture Cure for Conformal Coatings
Hi Technetters,
I work for a company that manufactures Ovens for curing conformal coatings
and recently we have received a few requests for ovens that can regulate the
relative humidity inside the process cavity of the oven to approximately 50%
. While researching this application we have found that the moisture cure is
needed for some silicon coatings to activate or accelerate the cure.
What I am wondering is how much need their is in this market for such a
system. I don't think any other oven manufacturers offer such a system so I
am wondering what other people in the industry are currently doing to meet
this RH Requirement? Are they using a normal oven and modifying it somehow
to meet these needs or ??? If you are currently using a moisture cure
conformal coating or are a manufacturer of conformal coatings I would love
your imput.
I can be contacted offline at <[log in to unmask]> (e-mail) or 509-483-0900
(voice).
Thank you,
Brian Stumm
ETS, LLC
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body: To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information. For the technical support contact Dmitriy Sklyar at [log in to unmask]
org or 847-509-9700 ext.311
################################################################
-------- REPLY, End of original message --------
--
Tony Bugeja, P.Eng. E-Mail: [log in to unmask]
Process Engineer Phone: (204) 631-7241
C-Mac Electronics Fax: (204) 631-7294
1455 Mountain Ave
Wpg., Mb. R2X 2Y9
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|