     You are going to have trouble meeting all of the visual requirements 
     with hot bar attach. It is a side effect of the attach method. I had 
     to have special visual requirements for it, and these were not in any 
     standard. Maybe there is something now. I do not know.


______________________________ Reply Separator _________________________________
Subject: FWD>assy: hot bar solder jo
Author:  [log in to unmask] at internet
Date:    7/10/96 7:40 PM


this message is being forwarded from a co-worker,

the solder joints that we are forming with our hot bar process are not meeting
the requirements of 'standard' workmanship criteria.  in particular, we have a
difficult time meeting 'heel fillet' requirements.  the defect is one of
'insufficient solder' at the heel fillet.  it isn't that there isn't any heel
fillet; it's just that it isn't as pronounced as the standards require.

question.-  are there solder joint standards specific to hot bar soldering?

thanks,

phil crepeau, trw-san diego

Judy Murray
TRW San Diego
619.592.3616
[log in to unmask]

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2