TECHNET Archives

September 2002

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Earl Moon <[log in to unmask]>
Date:
Mon, 9 Sep 2002 08:16:48 -0500
X-To:
Joyce Koo <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Earl Moon <[log in to unmask]>
Parts/Attachments:
text/plain (29 lines)
Joyce,

Back in the old through hole days, when plating and fusing with peanut oil,
the surface condition was primo and lasted in military use for years. Of
course then we didn't know as much. Werner's comments on edge intermetallic
growth, and possible oxidation on the edges as the plating "pulls" back to
form the well known dome, make sense to me. However, my thoughts are of
going back in time, or doing it now, and using a modern hot air reflow oven
has me interested but the solder plating thickness would be a bit much using
the old plating process requirement I think was ,0003" minimum but maybe it
could be thinner now to achieve a flat surface.

I think Teledyne's old operation, before whoever bought them discontinued
using the process on component leads that soldered great, was the last to
use it. Nothing has been the same since.

Earl

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2