TECHNET Archives

December 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Sat, 4 Dec 1999 09:28:36 -0800
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Carey Pico <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
Carey Pico <[log in to unmask]>
Parts/Attachments:
text/plain (215 lines)
ECR is a vacuum process in being applied this way.  SiOx is not conductive
enough for a electrical contact coating.

Carey

-----Original Message-----
From: joyce <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Friday, December 03, 1999 6:35 PM
Subject: Re: [TN] anti-abrasion finish


>May be you should look into large area SiO2 deposition using ECR (electron
>cycletron resonance) process.  It is NOT high vacuum process and can be
used
>for large area coating (don't ask me how to rework or take it
off....)..Good
>luck.
>                                  jk
>At 08:09 AM 12/4/99 +1100, you wrote:
>>Carey I have no idea where Ralph is coming from (wet or dry process),
>>only thing understood was protection of metal .
>>You're quite correct, TiN coats are vacuum and vapor deposit,
>>nothing wet about it .
>>
>>Where did this wet note came from , Ralph did not mention any (neither
me).
>>You got me bit confused : know the application ?
>>Why did you highlight the refractory character ?
>>And, yes , big sheet coat is a process (and chamber) problem
>>
>>Paul
>>
>>-----Original Message-----
>>From: Carey Pico [mailto:[log in to unmask]]
>>Sent: Friday, 3 December 1999 10:33
>>To: [log in to unmask]
>>Subject: Re: [TN] anti-abrasion finish
>>
>>
>>Can you get a decent TiN coating with wet plating?  I thought that was a
>>vacuum process.
>>
>>Carey
>>-----Original Message-----
>>From: Paul Klasek <[log in to unmask]>
>>To: [log in to unmask] <[log in to unmask]>
>>Date: Thursday, December 02, 1999 2:46 PM
>>Subject: Re: [TN] anti-abrasion finish
>>
>>
>>>Why don't you try Ti Nitride coatings Ralph,
>>>there are 3-4 different colours/formulations (apart from the oldest
goldish
>>>one);
>>>they're relatively cheap, work superbly ;
>>>it's basically a ceramic coat, with mildly different hardness ratios .
>>>Metal finish is always inferior to ceramic coats ;
>>>and those nowadays go even to engines = quite common .
>>>Microcrystalline alumina is way out of any metal's reach ;
>>>as you're moving just below diamond ceiling in carborundum strata .
>>>
>>>You can also get the part sintered fully from ceramic compound,
>>>if possible/necessary/affordable = pending application
>>>
>>>Let me know if you get stuck or need more details,
>>>with application
>>>
>>>Paul Klasek (aka the carbon fan [as all of us])
>>>ResMed
>>>
>>>PS
>>>The cer coats being hard are fragile = you still need a very good (hard)
>>>base,
>>>and treat the part as an egg .
>>>Than the polish (lengthy, automated, as glass polish) = smooth surface,
>>will
>>>lengthen the life of the surface.
>>>Still, keep in mind you're in 9.th (10.th diamond) scale with alumina,
>>>don't expect infinite service .
>>>
>>>PPS
>>>The synthetic diamond has been formed in few labs,
>>>but we'd be in straight vertical stratosphere on $'s .
>>>
>>>NB
>>>Just hook on search engines with "ceramic coats" and "ceramic tool bit
(or
>>>tip)" ;
>>>should give you plenty options .
>>>Cer. tip could be the one for you
>>>
>>>
>>>-----Original Message-----
>>>From: Vaughan, Ralph H [mailto:[log in to unmask]]
>>>Sent: Friday, 3 December 1999 5:50
>>>To: [log in to unmask]
>>>Subject: [TN] anti-abrasion finish
>>>
>>>
>>>Hi TN,
>>>
>>>A follow-up query to a recent posting about sand-type abrasion for you
>>>metalheads (Dave H., you there?); Is there a metal finish that will
>>>withstand rubbing wear from aluminum oxide powder?  we have tried
tungstun
>>>carbide and stellite with 'no joy'.    Any light bulbs going on?
>>>
>>>Thanks for thinking
>>>
>>>Ralph Vaughan
>>>
>>>##############################################################
>>>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>>>##############################################################
>>>To subscribe/unsubscribe, send a message to [log in to unmask] with
following
>>>text in
>>>the body:
>>>To subscribe:   SUBSCRIBE TECHNET <your full name>
>>>To unsubscribe:   SIGNOFF TECHNET
>>>##############################################################
>>>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
>>additional
>>>information.
>>>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask]
or
>>>847-509-9700 ext.5365
>>>##############################################################
>>>
>>>##############################################################
>>>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>>>##############################################################
>>>To subscribe/unsubscribe, send a message to [log in to unmask] with
following
>>text in
>>>the body:
>>>To subscribe:   SUBSCRIBE TECHNET <your full name>
>>>To unsubscribe:   SIGNOFF TECHNET
>>>##############################################################
>>>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
>>additional
>>>information.
>>>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask]
or
>>>847-509-9700 ext.5365
>>>##############################################################
>>>
>>
>>##############################################################
>>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>>##############################################################
>>To subscribe/unsubscribe, send a message to [log in to unmask] with
following
>>text in
>>the body:
>>To subscribe:   SUBSCRIBE TECHNET <your full name>
>>To unsubscribe:   SIGNOFF TECHNET
>>##############################################################
>>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
>>information.
>>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
>>847-509-9700 ext.5365
>>##############################################################
>>
>>##############################################################
>>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>>##############################################################
>>To subscribe/unsubscribe, send a message to [log in to unmask] with
following
>text in
>>the body:
>>To subscribe:   SUBSCRIBE TECHNET <your full name>
>>To unsubscribe:   SIGNOFF TECHNET
>>##############################################################
>>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
>>information.
>>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
>>847-509-9700 ext.5365
>>##############################################################
>>
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
>the body:
>To subscribe:   SUBSCRIBE TECHNET <your full name>
>To unsubscribe:   SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
>information.
>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
>847-509-9700 ext.5365
>##############################################################
>

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2