It says "no clean" and therefore one would think that you do not have to clean it.  The IPC standards says that residue from no clean fluxes are acceptable provided it has been qualified and documented by your process engineer as benign.  It has been my
experience that some "no clean" fluxes have corrosion issues.  If I were you I would do some ionic testing.  Check out IPC -TM-650 for test procedures.  You might also check the chemical content of the flux you're using.  If it contains halides then you
most likely have a problem.  Good luck!
Dyane White
Technical/Process Trainer
Philips Ultrasound
Bothell, WA


                                                                                                                           
                    Olivia Mc Dermott                                                                                      
                    <oliviamcdermott01@HO           To:  [log in to unmask]                                                   
                    TMAIL.COM>                      cc:  (bcc: Dyane White/ATL-BTL/MS/PHILIPS)                             
                    Sent by: TechNet                Subject:  [TN] Flux residue with a no-clean process                    
                    <[log in to unmask]>                                                                                      
                                                    Classification:                                                        
                                                                                                                           
                    01/30/02 05:48 AM                                                                                      
                    Please respond to                                                                                      
                    "TechNet E-Mail                                                                                        
                    Forum."; Please                                                                                        
                    respond to Olivia Mc                                                                                   
                    Dermott                                                                                                
                                                                                                                           
                                                                                                                           




Is it OK to have flux residue on assemblies when the process is no clean. We
have assemblies that are failing in the field and the customer thinks this
flux residue may be an issue. They think the assembly has been wet.
What do you think???? All help appreciated.

_________________________________________________________________
Join the world's largest e-mail service with MSN Hotmail.
http://www.hotmail.com

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------



---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2