Parts/Attachments:
text/plain (66 lines)
HELLO GUYS,
   
  WE NEED A VACUM CHAMBER FOR UNIVERSITY BASED RESEARCH EXPERIMENT.
  ANY ONE OUT THERE HAS A OLD ONE WANTS TO TO GET RID OF?
   
  PLEASE LET ME KNOW IF YOU KNOW A REASONABLE ONE TOO.
   
  YOURS,
  AL
   
  

Bev Christian <[log in to unmask]> wrote:
  Technetters,
Good morning! We generally do not use PTH parts. As a result, we do
not do wave soldering, but use paste-in-hole or pin-in-paste, chose your
moniker. Because we buy the part in question from two different
suppliers, who make the parts with different dimensions, we have had to
use fairly large, oval holes instead of a more conventional round hole.
And the part leads do not stick out the bottom of the hole either. With
overprinting we have been able to get what is deemed adequate solder
joint strength (and reliability (Yes, I know the difference, Werner.)),
even though the hole fill is not stellar. Wetting angles are good and
proper intermetallics are formed.

Now let's say we do a rework - removing the component, dressing the
hole, inserting a new part and resoldering using hand soldering with
cored wire. The internal debate is whether we should demand hole fill
to meet normal IPC standards or whether we allow the same amount of hole
fill that is allowed for the original paste-in-hole. Opinions and/or
experiences (if you are willing to share the latter :) ) appreciated.
Thanks in advance.

Bev 
RIM



---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------


       
---------------------------------
Need a vacation? Get great deals to amazing places on Yahoo! Travel. 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2