Roger,

Why do your customers want to use contact cleaners/lubricants for IC
sockets?  Is there a specific problem they think they're having which they
think this material will solve?  I have used these materials only as
band-aids to help fix high insertion force and fretting corrosion issues
with IC sockets.  I say "band-aid" because they didn't address the root
cause of the problems, primarily incorrect socket selection, IC lead
material selection and board cleaning.

On other types of contacts/sockets, I think these types of materials are
fine.

Caig labs (http://www.caig.com) should be able to help you answer any
technical issues with their DeOxit product.

-- Gregg
[log in to unmask]


At 07:30 AM 12/10/99 -0600, Roger Hill wrote:
>    Does anyone have any opinions on the use of contact  cleaners/enhansers?
>Many of our customers are asking if they can safely use  this (Deoxit is one
>  We are starting some testing to make sure  it will not attack the
>chip carrier plastic - but I thought I would ask the  group.
>
>Roger Hill
>[log in to unmask]

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2