Roger,
Why do your customers want to use contact cleaners/lubricants for IC
sockets? Is there a specific problem they think they're having which they
think this material will solve? I have used these materials only as
band-aids to help fix high insertion force and fretting corrosion issues
with IC sockets. I say "band-aid" because they didn't address the root
cause of the problems, primarily incorrect socket selection, IC lead
material selection and board cleaning.
On other types of contacts/sockets, I think these types of materials are
fine.
Caig labs (http://www.caig.com) should be able to help you answer any
technical issues with their DeOxit product.
-- Gregg
[log in to unmask]
At 07:30 AM 12/10/99 -0600, Roger Hill wrote:
> Does anyone have any opinions on the use of contact cleaners/enhansers?
>Many of our customers are asking if they can safely use this (Deoxit is one
> We are starting some testing to make sure it will not attack the
>chip carrier plastic - but I thought I would ask the group.
>
>Roger Hill
>[log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|