TECHNET Archives

June 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Kerry McMullen <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Mon, 26 Jun 2006 13:37:33 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (115 lines)
What is a Bellville washer?
TIA

Kerry McMullen
Principal New Product Mfg. Engineer
LTX Corporation
50 Rosemont Road
Westwood, MA 02090-2306
(T) 781-467-5468



John Burke <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
06/26/2006 01:36 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
John Burke <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re: [TN] Plating Recomendation?






No comment about the finish, but you might recommend he use Bellville
washers on the bolt asseblies.

John

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Parsons
Sent: Monday, June 26, 2006 10:21 AM
To: [log in to unmask]
Subject: [TN] Plating Recomendation?

Happy Monday!



I have a customer (we are a fabricator) asking the following question;



"..we are looking at making a board that is intended to be bolted to some
batteries through 6mm and 8mm nuts and bolts. I was wondering if you have
any recommendations on what sort of plating should be on the pads these
nuts
are going to screw down onto? The batteries are fairly heavy and the
apparatus may be subject to some vibration and shock. Thanks for your
insight."



I am thinking HASL has been used for years in similar applications but
does
anyone have any experience or are there any studies on the matter?



Regards



John Parsons




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2