TECHNET Archives

October 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Victor Hernandez <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Thu, 31 Oct 2013 14:51:30 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (12 lines)
Fellow TechNetters:

   IPC-TM-650 # 2.6.8 for PCB/PWB with and w/o PTH.   I want to conduct a Solderability test for a piece of sheet metal plated over with nickel.   Can I preform horizontal or vertical Solderability test.

Victor,


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2