TECHNET Archives

August 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
"Barmuta, Mike" <[log in to unmask]>
Date:
Fri, 8 Aug 2003 15:23:56 -0700
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Barmuta, Mike" <[log in to unmask]>
Parts/Attachments:
text/plain (65 lines)
Hans: Contrary to popular belief polyester is resistant, with the exception
of acids, to most chemicals including traditional "solvents". That's why
there are still so many of those old polyester suits still around from the
late 60's early 70's, you can't destroy the stuff.
As I recall a solution of 25% sodium hydroxide will break it down, conc.
propylene glycol may also work. You may want to try a little agitation and
heat to speed it up.

                                                                Good Luck!


Michael Barmuta

Staff Engineer

Fluke Corp.

Everett WA

425-446-6076




-----Original Message-----
From: Hans Shin [mailto:[log in to unmask]]
Sent: Friday, August 08, 2003 1:55 PM
To: [log in to unmask]
Subject: [TN] polyester


Does anyone know what solvents I can use to dissolve polyester (e.g.
polyethylene terepthalate, PET)?  I tried acetone, and quite a few other
solvents which should dissolve that stuff, but without any luck.  We are not
allowed to use acid.

Hans Shin
Pacific Testing Laboratories, Inc.
www.pacifictesting.com

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2