That's the only reason they make Scotch 600. It's been the industry standard coating adhesion test for over 50 years now!
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Lamar Young
Sent: Thursday, January 30, 2014 1:22 PM
To: [log in to unmask]
Subject: [TN] Tape for adhesion testing
ASTM D-3359 is the cross cut adhesion test method that is fairly common in the coating industry.
IPC TM-650 2.4.1.6 is a similar cross cut adhesion test method.
The ASTM called out the use of P-99 tape that was discontinued approximately 5 years ago. The ASTM committee last reported in 2010 that they were still evaluating replacement tapes.
The IPC TM-650, created in 1995, calls out 3M #600 as a suitable tape.
I was curious if most are using the #600 or a different tape (please specify).
The tape choice question surfaced during a discussion with a customer that originally specified a different tape.
I thought I'd ask others in the industry to better understand what tape the majority of the industry was using.
Thanks for your replies,
Lamar Young
Specialty Coating Systems, Inc.
7645 Woodland Dr.
Indianapolis, IN 46278
(317) 244-1200 Ext. 276
www.scscoatings.com
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|