Dear Dan,

Yes, we have experienced a dulling effect on solder joints using a batch
cleaner and a sapponifier in the past.  We wrestled with the problem for
a long time and eventually found that using an Armakleen formulation
with a built in brightener solved the problem.  It is important to
remember that a dull joint does not reduce joint reliability, only the
asthetic appearance.      

[log in to unmask]


___________________Reply Reparator______________________
Has anyone experienced dull, dark gray SMT solder joints after cleaning?
I am using a dishwasher and a neutralizer could these be the problems??

||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
    Dan Sadley                 
 [log in to unmask] 
3660 Quakerbridge rd.    
Trenton, NJ 08619         
(609) 587-9897 x-179     
 Fax (609) 587-1970        
||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2