Hi Colin,
Component long term storage was an investigation the NPL covered a few years
ago. Check out their website for report titled 'Shelf life & Solderability
ageing', It's is on free issue.
Regards,
Iain.
-----Original Message-----
From: Colin Weber [mailto:[log in to unmask]]
Sent: 20 March 2006 04:33
To: [log in to unmask]
Subject: [TN] Component Long Term Storage
*** WARNING ***
This mail has originated outside your organization,
either from an external partner or the Global Internet.
Keep this in mind if you answer this message.
Hello Folks,
Could anyone please advise on what realistic long term storage (many years)
can
be achieved, and how to achieve it, for components such as integrate
circuits?
Any articles or guidelines would be helpful.
We are facing some obsolete component issues and do not have resources to
redesign many boards for incompatible replacements or new devices.
After searching the archives I have ascertained that it seems the
hygroscopic
nature of the packages is not a great problem. J-STD-033 should help with
determining storage requirements for this issue. Would it be true to say
baking
the components can eliminate any absorbed moisture, even after many years of
long term storage?
A bigger problem appears to be intermetallic growth on the legs, between the
coating (tinning) and the actual leg material. The intermetallic can grow
over
time, eventually causing the legs to lose solderability. I suspect the
growth
rate is temperature dependent and could be slowed by cooling.
Regards,
Colin Weber
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
********************************************************************
This email and any attachments are confidential to the intended
recipient and may also be privileged. If you are not the intended
recipient please delete it from your system and notify the sender.
You should not copy it or use it for any purpose nor disclose or
distribute its contents to any other person.
********************************************************************
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|