TECHNET Archives

July 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Tom P. Hummel" <[log in to unmask]>
Date:
Thu, 12 Jul 2007 14:43:25 +0300
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Subject:
From:
Brian Ellis <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset=ISO-8859-15; format=flowed
MIME-Version:
1.0
Parts/Attachments:
text/plain (66 lines)
I don't know how many times it has been said here that a so-called 
"no-clean" flux is formulated primarily so that the residues are as 
benign as possible WITHOUT any cleaning process. If you choose to clean 
them, the residues may be much less benign. Fluxes that are designed to 
be cleaned are formulated to ensure the cleaning process is as easy as 
possible. I do not advise mixing types on any one assembly because you 
are negating that advantages of both. The easiest way round your problem 
is to use a water-soluble flux for wave soldering (and reduce your 
retouch rate at the same time!)

Brian

Tom P. Hummel wrote:
> Fellow TechNetters,
> 
>  
> 
> We are experiencing a white residue on the solder side of some boards
> after going through our wash system.  We are wave soldering the boards
> on a SeHo wave solder machine using Aim NC-264-5 no clean flux.  The
> boards have some additional components installed by hand using water
> soluble flux/solder.  The boards are then run through our Aqueous
> Technologies SMT series board washer.  When they complete the drying
> cycle, there is a white residue on the solder side of the boards that is
> very difficult to remove.  Has anyone else seen this residue from
> washing a board after using no clean flux?  Does anyone have any
> recommendations to help eliminate the residue?
> 
>  
> 
>  
> 
> Thomas P. Hummel
> 
> Carlton Industries Corp
> 
>  
> 
>  
> 
>  
> 
>  
> 
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
> 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2