Agreed!
The sprayed flux volume is critical to effective soldering, being able to
measure and control it is extremely important. It's almost amazing how many
reputable assembly companies do not understand the effect of too much or too
little flux and it's effect. The same goes for pre-heat.
Regards,
Andrew Hoggan
BBA Associates Ltd
www.bba-associates.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Alan Kreplick
Sent: 05 October 2001 13:17
To: [log in to unmask]
Subject: Re: [TN] SPC @ WAVE SOLDER
On a daily basis, I'm using a Wave Solder Optimizer (made by Technology
Information Corporation) for measuring preheat and wave dynamics (height,
width, parallelism).
On a monthly basis, I'm using a Spray Flux Fixture (made by
Vitronics-Soltec) for measuring flux volume sprayed.
I (the operators) track both with SPC software.
If used and understood, both tools are extremely valuable.
Al Kreplick
Sr. Mfg. Eng.
Teradyne, Inc.
500 Riverpark Drive
North Reading, MA 01864
Tel: 978-370-1726
Fax: 734-661-5352
(Embedded
image moved TechNet <[log in to unmask]>
to file: 10/04/2001 10:02 AM
pic00041.pcx)
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: [TN] SPC @ WAVE SOLDER
In regards to SPC at wavesolder. I would just like to here from some of the
people in this forum on what type of data they are collecting or sampling.
Any info is beneficial. Thanks.
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|