Morning An, we have successfully screen printed our vias closed. this was to
prevent conformal coating to leak to the other side. 1:1 aperture
We are having a couple boards via filled with silver paste by board house.
There are two conductive type, Methode makes one and Dupont makes another, I
do not know the numbers. Maybe someone else does.
Dave Chapman
Manufacturing Engineer
Circuit Service Inc.
-----Original Message-----
From: An [mailto:[log in to unmask]]
Sent: Monday, April 14, 2003 5:59 AM
To: [log in to unmask]
Subject: [TN] via filling
Hello,
I'm searching for information on filling of burried vias, blind vias, and
micro-vias. The more information I can find the better.
Which technology is available? Conductive or non-conductive? Plating or
screen-printing? Which suppliers?
Which process do you use? How are your experiences with it? For which
purposes do you fill?
I thank you in advance.
Sincerely
An gielen
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|