Hi Greg - I recommend you conduct a literature search for published papers
on the following project:
Electronic Miniaturization for Missile Applications (EMMA)
Time frame: October 2001
Funding Agency: American Competitiveness Institute
A QFN style device was included in the EMMA study which conducted both IPC
Class 3 thermal cycle and vibration testing as part of their assessment
program of SMT components. The data you are looking for is included in the
EMMA reports. Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
"Temkin, Gregg" <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
07/30/2008 04:26 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Temkin, Gregg" <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] Use of QFN devices in high reliability applications
Our team is working on several new electronic devices whose application is
primary, flight critical hardware for commercial aircraft.
Our initial component selection includes many QFN packaged devices
(leadless, bottom side termination only) which will be mounted on .063"
FR4 boards using SN63. The devices range from 20 to 44 terminations.
From studies that are available on the web, a picture has emerged that QFN
packages have reduced long term solder joint reliability when compared
with leaded or some of ball grid array devices. Board thickness, flexing
and whether the device has a central solderable heat sink seem to have a
significant affect on reliability. Problem is there are no absolute
numbers, so for critical applications it seems that thorough testing is
required. We'd rather not wait until the end of a lengthy test regimen to
find we've gone down the wrong path. Is there newer information
abbailable? Two of the studies stated that further testing was being
performed to support the reliability requirements for aerospace and other
high-rel applications however I cannot find any updated information on the
web.
We have decided to replace several of the QFN's with leaded devices,
however there are no direct crosses for 3 of the devices. One of them will
require a number of components to create the same function; possibly an
additional circuit card.
Is anyone aware of information or recommendations that would be useful for
our assessment? Is there any specific information that would drive us to
use or not use them?
Thanks for your help
Gregg
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|