Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0wm00F-000BleC; Wed, 9 Jul 97 11:54 CDT |
Content-Type: |
text/plain; charset=ISO-8859-1 |
Old-Return-Path: |
|
Date: |
Wed, 9 Jul 1997 13:03:18 -0400 |
Precedence: |
list |
Reply-To: |
|
Resent-Sender: |
|
MIME-Version: |
1.0 |
Status: |
O |
X-Mailing-List: |
|
X-Status: |
|
TO: |
|
X-Loop: |
|
Return-Path: |
<TechNet-request> |
Resent-From: |
|
X-Priority: |
3 |
Content-Transfer-Encoding: |
7bit |
From [log in to unmask] Wed Jul 9 13: |
49:24 1997 |
Resent-Message-ID: |
<"EpANb2.0.suH.j8ymp"@ipc> |
Subject: |
|
From: |
|
X-MSMail-Priority: |
Normal |
>From willli Wed Jul 9 11: |
54:40 1997 |
X-Mailer: |
Microsoft Internet Mail 4.70.1161 |
Message-Id: |
|
Parts/Attachments: |
|
|
In formulating solder masks I found that both the ionic contamination level
as well as minor improvement in pencil hardness is found. The UV bump can
be either before or after the thermal step. There are advantages to ethier
place.
----------
> From: [log in to unmask]
> To: [log in to unmask]
> Subject: U.V. cure of L.P.I. soldermasks
> Date: Wednesday, July 09, 1997 10:51 AM
>
>
>
>
>
>
>
> I have a question in regard to the curing of L.P.I.
> soldermasks. Many people cure their screened boards thermally only,
> with no U.V. "bump". Other people insist that the additional U.V.
> cure is needed to make the mask stronger 'pencil strength scale".
> Some people claim that the amount of hardness that the U.V. cure adds
> is so insignifigant to a properly thermally cured board, that it is a
> waste of valuable time to perform this operation. I am looking for
> some input on what other people have found in regard to this issue and
> would greatly appreciate any feedback that I can get. Thank you.
>
>
***************************************************************************
> * TechNet mail list is provided as a service by IPC using SmartList v3.05
*
>
***************************************************************************
> * To subscribe/unsubscribe send a message <to: [log in to unmask]>
*
> * with <subject: subscribe/unsubscribe> and no text in the body.
*
>
***************************************************************************
> * If you are having a problem with the IPC TechNet forum please contact
*
> * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]
*
>
***************************************************************************
>
>
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|