George: Type III chromate conversion coatings really don't offer much
environmental protection.
However they do offer some protection as opposed to straight zinc. Are the
fingerprints reacting and etching into the zinc plating or do they just show
up on the surface of the coating? I would expect a properly applied coating
to resist some handling.
Obviously a Salt Fog or Salt Spray test would help to give you some
quantitative indication of the quality of the coating, but that takes time
and equipment.
You can also do a weight loss test by weighing the part, stripping the
coating and re-weighing. I've used this method on aluminum with class 1A
coatings with success. However the accuracy of this for very thin coatings
is not the greatest and may be difficult for stripping the coating from a
zinc substrate.
A spot test can also be done. This is strictly a qualitative test but has a
very high sensitivity to the presence of Chromate. It will not tell you the
quality of the coating but it will definitely tell you if any Chromate is
present. Make a solution of 0.1% B.W. diphenylycarbazide to reagent grade
methanol. Place a drop on the suspect part. If there is Chromate present it
will turn a brilliant violet color.
Good Luck
Michael Barmuta
Staff Engineer
Fluke Corp.
Everett WA
425-446-6076
-----Original Message-----
From: Wenger, George M. [mailto:[log in to unmask]]
Sent: Friday, May 02, 2003 12:26 PM
To: [log in to unmask]
Subject: [TN] Type 3 Chromate Conversion Coating
If a cold rolled commercial quality steel (per ASTM A366) assembly that is
zinc plated (0.0002" min per ASTM B633 Type 3) and supposed to be colorless
chromate conversion coated begins to show finger prints and surface tarnish
in a relatively benign environment, should you suspect that the chromate
conversion coating is missing or improperly applied? And secondly, is there
an analytical method to determine the presence and quality of the coating or
would one have to resort to Salt Fog testing
Regards,
George
George M. Wenger (908)-546-4531
Reliability Engineer
RF Power Amplifier Group
Andrew Corporation, 40 Technology Drive, Warren, NJ 07059
[log in to unmask]
----------------------------------------------------------------------------
-----------------------
This message is for the designated recipient only and may
contain privileged, proprietary, or otherwise private information.
If you have received it in error, please notify the sender
immediately and delete the original. Any unauthorized use of
this email is prohibited.
----------------------------------------------------------------------------
-----------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|