Greg,
There are several references for conformal coatings. A good one is
http://outgassing.nasa.gov/
Click on Low Outgassing and then choose Conformal Coating in the search
category. This lists all the coatings with a max. of 1.0% TML and a max.
of 0.10% CVCM's.
NASA-STD-8739.1A is a workmanship standard.
http://www.hq.nasa.gov/office/codeq/doctree/NASA_STD_8739_1_A.pdf
The Aerospace report no. TOR-2006(8583)-5236 is another that lists
requirements. Section 2240 is for coatings and refers to IPC-CC-830 and
MIL-I-46058C. This reports was prepared for the Space and Missile Systems
Center Air Force Space Command.
http://www.everyspec.com/USAF/TORs/TOR2006-8583-5236_3772/
Lamar Young
Specialty Coating Systems, Inc.
7645 Woodland Dr.
Indianapolis, IN 46278
(317) 244-1200 Ext. 276
www.scscoatings.com
From: Gregg Owens <[log in to unmask]>
To: <[log in to unmask]>
Date: 11/16/2011 04:20 PM
Subject: [TN] Spaceflight (NASA) Approved CC
Sent by: TechNet <[log in to unmask]>
Dear TechNetters:
I have returned to SpaceX and have been posed a question which some of you
should have quick answers for (obviously not a Doug "It depends"
question).
'
What are the NASA approved conformal coatings for spaceflight? I was
hoping to find a list in the NASA-STDs but didn't find a list. Replies are
most appreciated.
Thanks,
Gregg Owens
SpaceX
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|