Bill,
We have put turret terminals in both plated and unplated holes in the past
with equally good results. However, you probably will not get a solder
fillet topside due to the swaging. Don't need a fillet topside really, due
to mechanical retention. We tend to stay away from this lately due to the
xtra labor cost of swaging.
Roger M. Stoops, C.I.D., PCB Designer
Spectra Precision Inc./Trimble Navigation Ltd.
5475 Kellenburger Rd.
Dayton, OH 45424-1099 USA
Ph: 937.233.8921 or 937.233.4574 ext 288
Fax: 937.233.7511
"Kasprzak,
Bill (esd) To: [log in to unmask]
USX" cc:
<bkasprzak@MO Subject: [TN] Mounting turret terminals on circuit boards
OG.COM>
Sent by:
TechNet
<[log in to unmask]
ORG>
10/03/00
09:07 AM
Please
respond to
"TechNet
E-Mail
Forum.";
Please
respond to
"Kasprzak,
Bill (esd)
USX"
Good Morning:
I am curious to know if there is a "right" way for the following:
Standard .062 thick, two sided board where turret terminals are mounted.
The
boards are being soldered to NASA-STD-8739.3.
The active circuitry is on one side of the board. (on the side that the
terminal is swaged).
For the turret terminal locations only....
Does the "correct" board design call for a pad on one side of the board
without a plated thru hole and no topside pad?
Or.... Can you have a standard plated thru hole when mounting terminals?
Any and all responses appreciated !
Bill Kasprzak
Moog Inc.
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|