TECHNET Archives

August 2017

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Fri, 25 Aug 2017 14:13:12 +0000
MIME-version:
1.0
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
John Burke <[log in to unmask]>
Message-ID:
In-Reply-To:
<52135AE4151D8343B16989B2BFBED7DA011FA19B4874@pfc-dc01>
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
Parts/Attachments:
text/plain (30 lines)
	
		
		
	
		
		Dried (aka heated reflowed deactivated and polymerized) flux is definitely an issue.
Get a corrective action on the supplier to ensure it is removed the same as any other BGA device.
		

		Sent from my iPad Pro
	





On Fri, Aug 25, 2017 at 2:12 AM +0800, "Steven Kelly" <[log in to unmask]> wrote:










Hi All,
I have a new hi-density BGA connector I am trying to assemble. When the supplier makes the connector they "solder balls onto the pin" (lead free). We see dried flux on the balls and when we solder the connector we are getting a few joints with head in pillow. The connector manufacturer says the dried flux is not an issue - is this true? Thanks. Steve Kelly