Hello all,
I have some 6 layer rigid flex boards with discolored copper in the flex
area. If I look at the flex (after 2.5 hour bake and 2 reflow cycles), I see
a uniform amber area for most of the circuit along a .250" trace; however,
there are some areas that are significantly lighter and some that are
significantly darker than the majority of the area. I'm not sure if I should
be concerned with this state of being, so I guess I have a few questions.
- What is this? One of the darker ones appeared to have the coverlay
delaminated (2 mil acrylic adhesive over 1 oz copper), but the lighter ones
seem to have no problems.
- How can I tell if it's a problem or if it'll cause any end-use
difficulties (or delaminate during use)? I've taken some samples and run
them through our reflow oven 24 times, soaked them in water for 3 hours, and
run them through reflow 4 more times. So far, the dark ones look like
there's delam (as shown by cross section), and the light ones look ok.
- What can my fabricator do to avoid it (assuming it is a problem)? Are
there better adhesives to use (epoxies, etc.)?
- Would cross-hatching the .250" trace reduce the liklihood of occurance?
Should I need to do this, or should a fully in control fab process not cause
this?
Ok, thank you all for your kind assistance. I'm never sure if I'm alone out
there in my rigid-flex woes, so I'm interested to see responses.
Thanks,
Matt Sanders
Matthew Sanders
PCB/Metal Procurement Engineer, Trimble Navigation Ltd.
[log in to unmask]
Phone: (408) 481-7817
Fax: (408) 481-8590
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|