TECHNET Archives

February 2014

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "lduso - Diamond-MT.com" <[log in to unmask]>
Date:
Mon, 3 Feb 2014 17:27:25 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Message-ID:
Subject:
From:
"Whittaker, Dewey (EHCOE)" <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (76 lines)
Lotion with motion or ocean of emotion.
Dewey 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of lduso - Diamond-MT.com
Sent: Monday, February 03, 2014 10:16 AM
To: [log in to unmask]
Subject: Re: [TN] Wrist strap continuous monitoring

Oh yeah, lots of lotion. Especially in the winter.

Lloyd Duso
Diamond-MT
Plant Manager
(814) 535-3505
www.Diamond-mt.com


On Mon, Feb 3, 2014 at 12:09 PM, Stadem, Richard D. < [log in to unmask]> wrote:

> We have been using CM systems for esd wrist straps and mat monitoring 
> for at least 13 years. The only issue we had for constant alarms was 
> if the operator failed due to dry skin. We have taught them to 
> moisturize their wrist with approved skin cream such as R&R 
> Moisturizing ESD Lotion, and that has pretty much fixed the issue. No 
> other issues reported, the constant monitor system works much better 
> than depending on daily wrist strap checks.
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Kerr, Bryan (UK)
> Sent: Monday, February 03, 2014 10:31 AM
> To: [log in to unmask]
> Subject: [TN] Wrist strap continuous monitoring
>
> Hi Folks
>
> Any consensus on the usefulness of continuous wrist strap monitoring ? 
> I have been running a pilot line and have had a lot of problems due to 
> constant alarms. Can't, at the moment, figure out if this is just a 
> true reflection on variation in operator grounding or some failings in 
> the monitoring system. Any experiences out there ?
>
> Regards
>
> Bryan Kerr
> ********************************************************************
> This email and any attachments are confidential to the intended 
> recipient and may also be privileged. If you are not the intended 
> recipient please delete it from your system and notify the sender.
> You should not copy it or use it for any purpose nor disclose or 
> distribute its contents to any other person.
> ********************************************************************
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or 
> [log in to unmask]
> ________________
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or 
> [log in to unmask] 
> ______________________________________________________________________
>


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2