Hi Judy:
Solder joints are solder joints - a reliable solder joint should not
be process specific although some processes are more suited to making
certain solder joint geometry's than others. The heel fillet is a
critical location for good solder joint reliability. I think that
meeting the "standard" requirements is not the issue - does the heel
fillet you end up with provide the reliability needed for the use
environment that you are in? If it does then document those facts for
internal or customer review. I would also suggest that you forward
that documentation/information (if you are allowed) to the IPC
ANSIJ-STD-001 committee so that the information can be incorporated
into the specification.
Dave Hillman
Rockwell Collins
[log in to unmask]
______________________________ Reply Separator _________________________________
Subject: FWD>assy: hot bar solder jo
Author: [log in to unmask] at ccmgw1
Date: 7/10/96 7:26 PM
this meesage is being forwarded from a co-worker,
the solder joints that we are forming with our hot bar process are not meeting
the requirements of 'standard' workmanship criteria. in particular, we have a
difficult time meeting 'heel fillet' requirements. the defect is one of
'insufficient solder' at the heel fillet. it isn't that there isn't any heel
fillet; it's just that it isn't as pronounced as the standards require.
question.- are there solder joint standards specific to hot bar soldering?
thanks,
phil crepeau, trw-san diego
Judy Murray
TRW San Diego
619.592.3616
[log in to unmask]
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
|
|
|