Hi Jan -
Try adding a small amount of solder paste on the shield's thru holes
and the joints should not be insufficient. The solder paste reflows as
the assembly hits the wave.
Dave Hillman
Rockwell Collins
[log in to unmask]
______________________________ Reply Separator _________________________________
Subject: FAB: Solder plated shields
Author: [log in to unmask] at ccmgw1
Date: 7/31/96 4:57 PM
Hi all!
I'm just curious. Is there any one who solder shields in their wave
solder machine?
We're soldering shields in our machine using some extra flux and a
little higher wave section at that moment on the pcb. But there's a
problem, we can't solder just one part. If you imagine that you have 2
exactly similar shields on a PCB, one shield going short ended and one
long sided going through the waves, and the shield which goes short
ended first won't solder one of the short sides, always. We've checked
if they're warped and so on, with no luck.
Any suggestions, ideas or anyone having similar problems, i sure would
appreciate them.
Regards,
Jan Merstrand
[log in to unmask]
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
|
|
|