It depends of course on the solder temperature, solder exposure time and
the AgPd thickness. We have soldered to AgPd pads, and the solder
exposure time was set to a few seconds. The AgPd was as thick as some
25 micrometers. Thickfilm fellas talk about 'leaching'.
Inge
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Guenter Grossmann
Sent: den 3 juli 2008 14:00
To: [log in to unmask]
Subject: [TN] Antw: [TN] Silver-Palladium termination SMT solder
problems
Grant
You have the same effect when soldering with tin lead. AgPd terminations
are not intended to be soldered. The surface is optimised to be fixed
with adhesive. AgPb solves very easy in tin alloys. The effect is that
the entire metallisation is solved in the solder. The alloy that forms
looks as if you had a bad wetted solder joint. If you have a
,microsection done you will see that the AgPd metallisation has mostly
gone into the solder, in extreme cases exposing the ceramic of the
capacitor.
Best regards
Guenter
_____________________________________________________
EMPA
Swiss Federal Laboratories for Materials Testing and Research Centre
for Reliability Guenter Grossmann, Senior Engineer
8600 Duebendorf
Switzerland
Phone: xx41 44 823 4279
Fax : xx41 44 823 4054
mail: [log in to unmask]
_____________________________________________________
>>> Grant Emandien <[log in to unmask]> 07/02/08 11:19 am >>>
Hi all,
We are experiencing poor solderability with AgPd-terminations on MOVs
exposed to a lead-free reflow profile using a SAC alloy on an
ENIG-finished PCB. Though we have run this board only once previously
with the same part finish using a lead-rich alloy, we had similar
effects but not to the extent we are now experiencing.
Can anyone provide some insight into this/
Regards
Grant
**********************************************************************
Relevant company disclaimers are available at the following addresses:
Tellumat (Pty) Ltd e-mail:
mailto:[log in to unmask]
Web: http://www.tellumat.com/email.aspx
**********************************************************************
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|