I would expect so. Methanol is an alcohol and would have similar wetting
(or greater) than for isopropanol.
Doug Pauls
Principal Materials and Process Engineer
Rockwell Collins
On Fri, Apr 24, 2015 at 10:12 AM, Nutting, Phil <[log in to unmask]>
wrote:
> We have had many posts regarding the ability of alcohol to evenly
> distribute flux and other contaminates over the surface of the board or
> part. Does methanol do that same thing?
>
> Phil Nutting | HVP Development Engineer | Excelitas Technologies Corp
>
> Lab: +1 978.224.4332 | Office: +1 978.224.4152
> 35 Congress St, Salem, MA 01970 USA
> [log in to unmask]<mailto:[log in to unmask]>
> www.excelitas.com<http://www.excelitas.com/>
>
>
> [Excelitas R_emailsig]
>
>
> Please consider the environment before printing this e-mail.
> ________________________________
> This email message and any attachments are confidential and proprietary to
> Excelitas Technologies Corp. If you are not the intended recipient of this
> message, please inform the sender by replying to this email or sending a
> message to the sender and destroy the message and any attachments. Thank
> you.
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|